Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.05 g/cm³ Show Material materials with Dichte of 1.05 g/cm³ | |
Wasserabsorption | 23.0 °C | 0.04 % Show Material materials with Wasserabsorption of 0.04 % | ASTM D570, 24h equilibrium |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 71 MPa Show Material materials with Biegefestigkeit of 71 MPa |
Biegemodul | 23.0 °C | 39 GPa Show Material materials with Biegemodul of 39 GPa |
Elastizitätsmodul | 23.0 °C | 3.4 GPa Show Material materials with Elastizitätsmodul of 3.4 GPa |
Elongation at yield | 23.0 °C | 1 % Show Material materials with Elongation at yield of 1 % |
Streckgrenze | 23.0 °C | 41 MPa Show Material materials with Streckgrenze of 41 MPa |
Zugfestigkeit | 23.0 °C | 41 MPa Show Material materials with Zugfestigkeit of 41 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 99.85 °C Show Material materials with Glasübergangstemperatur of 99.85 °C | ||
Heat deflection temperature, 1.80 MPa | 98.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 98.85 °C | ||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.2E-5 1/K | |
Max. Betriebstemperatur | 126.85 °C Show Material materials with Max. Betriebstemperatur of 126.85 °C | ||
Schmelzpunkt | 269.85 °C Show Material materials with Schmelzpunkt of 269.85 °C | DSC | |
Schmelzwärme | 53 J/g Show Material materials with Schmelzwärme of 53 J/g |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.6 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 2.6 [-] | |
Surface resistivity | 23.0 °C | 1.00E+14 Ω/sq Show Material materials with Surface resistivity of 1.00E+14 Ω/sq | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Thermoplastics is used for automobile parts, electrical and electronic parts. |