Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.05 % Show Material materials with Wasserabsorption of 0.05 % | ASTM D570, 24h equilibrium |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 166 MPa Show Material materials with Biegefestigkeit of 166 MPa |
Biegemodul | 23.0 °C | 97 GPa Show Material materials with Biegemodul of 97 GPa |
Elastizitätsmodul | 23.0 °C | 10 GPa Show Material materials with Elastizitätsmodul of 10 GPa |
Elongation at yield | 23.0 °C | 1.5 % Show Material materials with Elongation at yield of 1.5 % |
Streckgrenze | 23.0 °C | 121 MPa Show Material materials with Streckgrenze of 121 MPa |
Zugfestigkeit | 23.0 °C | 121 MPa Show Material materials with Zugfestigkeit of 121 MPa |
Thermisch
Property | Temperature | Value | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 248.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 248.85 °C | ||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 1/K | |
Max. Betriebstemperatur | 126.85 °C Show Material materials with Max. Betriebstemperatur of 126.85 °C | ||
Schmelzpunkt | DSC |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.9 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 2.9 [-] | |
Surface resistivity | 23.0 °C | 1.00E+14 Ω/sq Show Material materials with Surface resistivity of 1.00E+14 Ω/sq | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Thermoplastics is used for automobile parts, electrical and electronic parts. | |
Fillers | Glass Fiber |