Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastizitätsmodul | 73.0 - 80.0 GPa Show Material materials with Elastizitätsmodul of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Zugfestigkeit | 325.0 MPa Show Material materials with Zugfestigkeit of 325.0 MPa | Pink Sheets, ASTM B686 | Casting |
Thermisch
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300 °C | 0.0000229 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000229 1/K | derived value for 20-300°C | ||
Schmelzpunkt | 546.0 - 621.0 °C Show Material materials with Schmelzpunkt of 546.0 - 621.0 °C | Pink Sheets, ASTM B686 | Casting | ||
Spezifische Wärmekapazität | 100 °C | 963 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963 J/(kg·K) | unstated value | ||
Wärmeleitfähigkeit | 23 °C | 128 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 128 W/(m·K) | unstated value |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.20 % Show Material materials with Eisen of 0.20 % | Pink Sheets, ASTM B686 | Casting |
Kupfer | 1.6 - 2.0 % Show Material materials with Kupfer of 1.6 - 2.0 % | Pink Sheets, ASTM B686 | Casting |
Magnesium | 0.4 - 0.6 % Show Material materials with Magnesium of 0.4 - 0.6 % | Pink Sheets, ASTM B686 | Casting |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | Pink Sheets, ASTM B686 | Casting |
Silizium | 8.6 - 9.4 % Show Material materials with Silizium of 8.6 - 9.4 % | Pink Sheets, ASTM B686 | Casting |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | Pink Sheets, ASTM B686 | Casting |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | Pink Sheets, ASTM B686 | Casting |