Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 73.0 - 80.0 GPa Show Material materials with Elastizitätsmodul of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 0.0000209 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000209 1/K | nominal value between 20°C and the mentioned temperature |
300 °C | 0.0000229 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000229 1/K | nominal value between 20°C and the mentioned temperature | |
Schmelzpunkt | 505.0 - 770.0 °C Show Material materials with Schmelzpunkt of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium | |
Spezifische Wärmekapazität | 100 °C | 963 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963 J/(kg·K) | unstated value |
Wärmeleitfähigkeit | 25 °C | 113 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 113 W/(m·K) | unstated value |