Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 - 25 % Show Material materials with Dehnung of 20 - 25 % |
Zugfestigkeit | 23.0 °C | 350 - 380 MPa Show Material materials with Zugfestigkeit of 350 - 380 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: Hot formed and machined parts for water fittings and other fluid handling systems where mildly acid or alkali solutions may be found | |
Corrosion properties | Good corrosion resistance |