Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.5 g/cm³ Show Material materials with Dichte of 7.5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 - 12 % Show Material materials with Dehnung of 10 - 12 % |
Streckgrenze Rp 0,2 | 23.0 °C | 320 - 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 320 - 400 MPa |
Zugfestigkeit | 23.0 °C | 650 - 700 MPa Show Material materials with Zugfestigkeit of 650 - 700 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 0-300°C |
Schmelzpunkt | 1060 - 1075 °C Show Material materials with Schmelzpunkt of 1060 - 1075 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 59 - 67 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 59 - 67 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 6.96E+6 - 8.12E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 6.96E+6 - 8.12E+6 S/m |
Specific Electrical conductivity | 12 - 14 % IACS Show Material materials with Specific Electrical conductivity of 12 - 14 % IACS |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.5 [-] Show Material materials with Relative magnetische Permeabilität of 1.5 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 8.5 - 11 % Show Material materials with Aluminium of 8.5 - 11 % | ||
Eisen | 4 - 5.5 % Show Material materials with Eisen of 4 - 5.5 % | ||
Kupfer | Balance | ||
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % | max. | |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Valve and pump components, marine hardware and high strength fasteners;Aerospace: High strength fasteners, springs, thrust washers and bearing bushes;Other: Gears, bearing races, valve stems, valve seats, worm gears, bearings, bushes, cams, pump rods and safety tools | |
Corrosion properties | Very high resistance to erosion and corrosion |