Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 - 13 % Show Material materials with Dehnung of 10 - 13 % |
Härte, Brinell | 23.0 °C | 200 - 220 [-] Show Material materials with Härte, Brinell of 200 - 220 [-] |
Streckgrenze | 23.0 °C | 400 - 500 MPa Show Material materials with Streckgrenze of 400 - 500 MPa |
Zugfestigkeit | 23.0 °C | 700 - 760 MPa Show Material materials with Zugfestigkeit of 700 - 760 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware, fasteners and fittings;General: Fasteners, gears, non-sparking safety tooling, thrust washers, valve guides, fluid handling equipment, valve spindles and components, bearings pins and bushes, thermostatic valves and worm wheels | |
Corrosion properties | Excellent general corrosion resistance | |
General machinability | Excellent machinability |