Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
BS C103 / Cu-OF Oxygen-free Copper
C103 (Cu-OF) is a commercially pure grade of oxygen-free copper manufactured by pouring in a protective gas atmosphere or vacuum. The absence of oxygen ensures high levels of electrical conductivity and low susceptibility to embrittlement when heated in a reducing atmosphere.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Suppliers with similar grades
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value | Comment |
---|---|---|
Kupfer | 99.95 % Show Material materials with Kupfer of 99.95 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | General: Radar and other electronic equipment, anodes for vacuum tubes, glass to metal seals in electronic equipment, thermostatic control valves, rotor conductors for large generators and motors, electrical equipment for service at elevated temperatures in the presence of reducing gases and anodes for electroplating, particularly in cyanide baths |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.