Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
BS C107 / Cu-DPA Arsenical Copper
2.1491 (CuAsP) is a copper alloy with a small addition of arsenic which enhances tensile strength properties at elevated operating temperatures up to 300°C. As well as increasing the softening resistance, the arsenic also enhances corrosion resistance in specific environments. This grade is deoxidised, which gives it freedom from hydrogen embrittlement, making it ideal for applications requiring welding and brazing. C107 has excellent fabrication characteristics and is typically specified for boiler plates and stay bolts in steam locomotive fireboxes. It shows the following features and properties:
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationThermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C |
Chemical properties
Property | Value |
---|---|
Arsen | 0.3 - 0.5 % Show Material materials with Arsen of 0.3 - 0.5 % |
Eisen | 0.03 % Show Material materials with Eisen of 0.03 % |
Kupfer | Balance |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Rail: Steam locomotive staybolts, rivets and boiler plates;Chemical processing: Chemical plant and equipment for relatively non-corrosive liquids and gases at moderately elevated temperatures | |
Corrosion properties | Good corrosion resistance |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.