Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 27 - 30 % Show Material materials with Dehnung of 27 - 30 % |
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa |
Härte, Brinell | 23.0 °C | 80 - 120 [-] Show Material materials with Härte, Brinell of 80 - 120 [-] |
Schubmodule | 23.0 °C | 56 GPa Show Material materials with Schubmodule of 56 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 125 MPa Show Material materials with Streckgrenze Rp 0,2 of 125 MPa |
Zugfestigkeit | 23.0 °C | 310 - 330 MPa Show Material materials with Zugfestigkeit of 310 - 330 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 29 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.90E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 2.90E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS | |
spezifischer Widerstand | 23.0 °C | 3.4E-7 Ω·m Show Material materials with spezifischer Widerstand of 3.4E-7 Ω·m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Salt water flanges, salt water piping and pipe fittings, valve bodies, sea water intakes, pipe fittings, water boxes, propeller sleeves, pump bodies and parts;Chemical processing: Heat exchanger and cooling plant, evaporator tubes, distiller tubes, refrigerator and condenser components;Other: Welding backing rings, flexible metal hose, weld wire and boiler parts | |
Cold Forming | Good cold formability | |
Corrosion properties | Excellent corrosion and pitting resistance in marine environments | |
General machinability | Easily machined, Machinability rating: 20 | |
Hot forming | Good hot formability with hot working temperature between 925-1025°C. |