Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.53 g/cm³ Show Material materials with Dichte of 8.53 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 40 J Show Material materials with Charpy impact energy, V-notch of 40 J |
Dehnung | 23.0 °C | 18 - 22 % Show Material materials with Dehnung of 18 - 22 % |
Streckgrenze Rp 0,2 | 23.0 °C | 400 - 430 MPa Show Material materials with Streckgrenze Rp 0,2 of 400 - 430 MPa |
Zugfestigkeit | 23.0 °C | 710 - 725 MPa Show Material materials with Zugfestigkeit of 710 - 725 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | for 0-400°C |
Schmelzpunkt | 1030 - 1085 °C Show Material materials with Schmelzpunkt of 1030 - 1085 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 25 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 3.5E-7 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.01 [-] Show Material materials with Relative magnetische Permeabilität of 1.01 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1 - 2 % Show Material materials with Aluminium of 1 - 2 % | ||
Andere | 0.3 % Show Material materials with Andere of 0.3 % | max., Inosinic acid (IMP) | |
Chrom | 0.5 % Show Material materials with Chrom of 0.5 % | ||
Eisen | 0.7 - 1.2 % Show Material materials with Eisen of 0.7 - 1.2 % | ||
Kupfer | Balance | ||
Mangan | 3.5 - 5.5 % Show Material materials with Mangan of 3.5 - 5.5 % | ||
Nickel | 13.5 - 16.5 % Show Material materials with Nickel of 13.5 - 16.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Critical marine fasteners, gears, shafts, pipe couplings, sonar equipment, connectors, flanges and subsea components | |
Corrosion properties | Excellent corrosion and pitting resistance in marine environments | |
General machinability | Easily machined |