Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.5 g/cm³ Show Material materials with Dichte of 8.5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Elastizitätsmodul | 23.0 °C | 141 GPa Show Material materials with Elastizitätsmodul of 141 GPa |
Härte, Brinell | 23.0 °C | 229 - 240 [-] Show Material materials with Härte, Brinell of 229 - 240 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 555 - 630 MPa Show Material materials with Streckgrenze Rp 0,2 of 555 - 630 MPa |
Zugfestigkeit | 23.0 °C | 770 - 850 MPa Show Material materials with Zugfestigkeit of 770 - 850 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.64E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.64E-5 1/K | for 0-400°C |
Schmelzpunkt | 1080 - 1100 °C Show Material materials with Schmelzpunkt of 1080 - 1100 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 44 - 46 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 - 46 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.7E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.7E-7 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine shafts and bearing bushes, offshore bolting, valve and pump trim;Aerospace: Aircraft landing gear bushes, actuating sleeves, steering gear, bearing bushes, non-magnetic bolts and control surface components;Automotive: High performance engine shafts, gears, pinions, bearing bushes, locking nuts, mechanical and electromechanical components, thrust washers and hydraulic equipment;Chemical processing: Pump and valve spindles and other trim, flanges, pipe fittings, clamps and plant components | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Good machinability |