Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Härte, Brinell | 23.0 °C | 140 [-] Show Material materials with Härte, Brinell of 140 [-] |
Härte, Vickers | 23.0 °C | 140 [-] Show Material materials with Härte, Vickers of 140 [-] |
Streckgrenze | 23.0 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical: Switchgear components, circuit breaker parts, rotating electrical machinery, electrical and thermal conductors;Chemical processing: Turbine generators, current-carrying arms and shafts for process plants;Other: Resistance welding, electrodes, shafts, electrode holders, seam welding wheels and flash or butt welding dies |