Mechanisch
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Chemical processing: Chemical process plant applications;Other: Furnace components to withstand oxidising, carburising and nitriding atmospheres, food processing, nuclear engineering and spark electrodes | |
Cold Forming | Excellent cold formability | |
Corrosion properties | High corrosion resistance | |
Hot forming | Excellent hort formability |