Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.44 g/cm³ Show Material materials with Dichte of 8.44 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 30 % Show Material materials with Dehnung of 30 % |
Elastizitätsmodul | 23.0 °C | 207 GPa Show Material materials with Elastizitätsmodul of 207 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 275 - 415 MPa Show Material materials with Streckgrenze Rp 0,2 of 275 - 415 MPa |
Zugfestigkeit | 23.0 °C | 690 - 830 MPa Show Material materials with Zugfestigkeit of 690 - 830 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.28E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.28E-5 1/K | for 0-100°C |
Schmelzpunkt | 1290 - 1350 °C Show Material materials with Schmelzpunkt of 1290 - 1350 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 9.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 9.8 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.32E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.32E-6 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % | |
Chrom | 22 % Show Material materials with Chrom of 22 % | |
Eisen | 2 % Show Material materials with Eisen of 2 % | |
Molybdän | 9 % Show Material materials with Molybdän of 9 % | |
Nickel | 58 - 61 % Show Material materials with Nickel of 58 - 61 % | |
Niobium | 3.5 % Show Material materials with Niobium of 3.5 % | Nb+Ta |
Tantal | 3.5 % Show Material materials with Tantal of 3.5 % | Nb+Ta |
Titan | 0.2 % Show Material materials with Titan of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Components where exposure to sea water and high mechanical stresses are required, oil and gas production where hydrogen sulphide and elementary sulphur exist at temperature in excess of 150C, flare stacks, hydrocarbon processing from tar-sand and oil-shale recovery projects;Chemical processing: Flue gas desulphurisation plant, flare stacks, offshore sour oil and gas production, waste incineration, phosphoric acid production and nuclear fuel processing | |
Corrosion properties | Very good corrosion resistance |