Alloy 718 Nickel Alloy (API 6A)

View suppliers (55)
Want to keep this datasheet? Save it now in your required format

Description

2.4668 (NiCr19NbMo) in the solution treated condition as per AMS 5662 and to the API 6A specification. AMS5662 is most suitable for heavy machining, forming or welding as it is in its most malleable state, whereas API 6A provides high strength while meeting the maximum hardness requirements of the NACE MR0175, MR0103 and ISO 15156-3 specifications for use in oil tools in corrosive environments. It shows the following features and properties:


  • Excellent tensile, fatigue, creep and rupture strengths across a wide temperature range from around -253ºC to 705ºC
  • Excellent oxidation resistance, up to temperatures of around 980ºC due to the high chromium content
  • Outstanding corrosion resistance in many environments including organic and inorganic acids, other than when strongly oxidising, hydrogen sulphide and sour gases
  • Especially resistant to chloride stress-corrosion cracking
  • Exceptional weldability
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    17 %

    Show Material materials with Dehnung of 17 %

    Härte, Brinell

    23.0 °C

    277 - 354 [-]

    Show Material materials with Härte, Brinell of 277 - 354 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    827 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 827 MPa

    Zugfestigkeit

    23.0 °C

    1034 MPa

    Show Material materials with Zugfestigkeit of 1034 MPa

    Chemical properties

    PropertyValue

    Aluminium

    0.5 %

    Show Material materials with Aluminium of 0.5 %

    Chrom

    19 %

    Show Material materials with Chrom of 19 %

    Eisen

    18 - 18.5 %

    Show Material materials with Eisen of 18 - 18.5 %

    Molybdän

    3 %

    Show Material materials with Molybdän of 3 %

    Nickel

    53 %

    Show Material materials with Nickel of 53 %

    Niobium

    5 %

    Show Material materials with Niobium of 5 %

    Titan

    0.9 %

    Show Material materials with Titan of 0.9 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Aerospace: Jet engine components, rocket motors and thrust reversers;Power generation: Nuclear reactor parts, gas turbine components, nuclear fuel element spacers, containment vessels and valves;Other: Hot extrusion tooling

    Cold Forming

    It can be cold worked while in the solution treated condition due to its high elongation.

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Readily machined in the solution treated condition but the material’s high strength and work-hardening characteristics should be taken into account.

    Hot forming

    It can be hot worked between 985-1150°C.