Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.47 g/cm³ Show Material materials with Dichte of 8.47 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Elastizitätsmodul | 23.0 °C | 100 GPa Show Material materials with Elastizitätsmodul of 100 GPa |
Härte, Vickers | 23.0 °C | 130 [-] Show Material materials with Härte, Vickers of 130 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 230 MPa Show Material materials with Streckgrenze Rp 0,2 of 230 MPa |
Zugfestigkeit | 23.0 °C | 520 MPa Show Material materials with Zugfestigkeit of 520 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 940 - 980 °C Show Material materials with Schmelzpunkt of 940 - 980 °C | |
Wärmeleitfähigkeit | 23.0 °C | 46 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 46 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.22E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.22E+6 S/m |
Specific Electrical conductivity | 9 % IACS Show Material materials with Specific Electrical conductivity of 9 % IACS | |
spezifischer Widerstand | 23.0 °C | 1.8E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.8E-7 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.05 [-] Show Material materials with Relative magnetische Permeabilität of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Blei | 1 - 2.5 % Show Material materials with Blei of 1 - 2.5 % | ||
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | max. | |
Kupfer | 44 - 47 % Show Material materials with Kupfer of 44 - 47 % | ||
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % | ||
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % | ||
Zink | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Frequently used applications of NS101 include gears, pinions, clock and watch parts, screws and other types of fasteners, hot stampings and forgings, keys, lock parts, door furniture, grills, decorative and architectural metalwork, darts, fishing tackle, camera, binocular and microscope parts, musical instrument valves and fittings, electrical and electronic pins and connectors and switchgear components. | |
Corrosion properties | Good corrosion resistance | |
General machinability | Very good machining and hot stamping characteristics |