Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.75 g/cm³ Show Material materials with Dichte of 8.75 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 45 % Show Material materials with Dehnung of 45 % |
Elastizitätsmodul | 23.0 °C | 135 GPa Show Material materials with Elastizitätsmodul of 135 GPa |
Härte, Vickers | 23.0 °C | 80 [-] Show Material materials with Härte, Vickers of 80 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa |
Zugfestigkeit | 23.0 °C | 390 MPa Show Material materials with Zugfestigkeit of 390 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 1060 - 1110 °C Show Material materials with Schmelzpunkt of 1060 - 1110 °C | |
Wärmeleitfähigkeit | 23.0 °C | 25 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.48E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 3.48E+6 S/m |
Specific Electrical conductivity | 6 % IACS Show Material materials with Specific Electrical conductivity of 6 % IACS | |
spezifischer Widerstand | 23.0 °C | 2.9E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.9E-7 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.05 [-] Show Material materials with Relative magnetische Permeabilität of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Blei | 0.03 % Show Material materials with Blei of 0.03 % | max. | |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % | max. | |
Kupfer | 60 - 65 % Show Material materials with Kupfer of 60 - 65 % | ||
Mangan | 0.05 - 0.5 % Show Material materials with Mangan of 0.05 - 0.5 % | ||
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % | ||
Zink | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | General: Architectural metalwork, panels and trim, holloware, musical instruments, medals and medallions, costume jewellery, nameplates, cosmetic cases, lamp caps, lighting fittings, platters, bowls, dials, relay and contact springs, medical, industrial and scientific instrument components | |
Cold Forming | Very good cold working characteristics | |
Corrosion properties | Excellent corrosion resistance |