Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.44 g/cm³ Show Material materials with Dichte of 8.44 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa |
Härte, Vickers | 23.0 °C | 185 [-] Show Material materials with Härte, Vickers of 185 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa |
Zugfestigkeit | 23.0 °C | 560 MPa Show Material materials with Zugfestigkeit of 560 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 850 - 870 °C Show Material materials with Schmelzpunkt of 850 - 870 °C | |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.90E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 2.90E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS | |
spezifischer Widerstand | 23.0 °C | 3.4E-7 Ω·m Show Material materials with spezifischer Widerstand of 3.4E-7 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.05 [-] Show Material materials with Relative magnetische Permeabilität of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Blei | 2.3 - 3.3 % Show Material materials with Blei of 2.3 - 3.3 % | ||
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % | max. | |
Kupfer | 47 - 50 % Show Material materials with Kupfer of 47 - 50 % | ||
Mangan | 1.5 - 3 % Show Material materials with Mangan of 1.5 - 3 % | ||
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % | ||
Zink | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | General: Gears, pinions, clock and watch parts, screws and fasteners, keys, lock parts, decorative and architectural metalwork, camera parts, electrical and electronic pins and connectors, medical, industrial and scientific instrument components | |
Corrosion properties | Very high corrosion resistance | |
General machinability | Excellent machinability |