Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.43 g/cm³ Show Material materials with Dichte of 4.43 g/cm³ | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Mechanisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Dehnung | 10 % Show Material materials with Dehnung of 10 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Elastizitätsmodul | 114.0 GPa Show Material materials with Elastizitätsmodul of 114.0 GPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Härte, Rockwell C | 36 [-] Show Material materials with Härte, Rockwell C of 36 [-] | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Zugfestigkeit | 895.0 - 931.0 MPa Show Material materials with Zugfestigkeit of 895.0 - 931.0 MPa | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Schmelzpunkt | 1674 °C Show Material materials with Schmelzpunkt of 1674 °C | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar | |
Spezifische Wärmekapazität | 370.0 - 674.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 370.0 - 674.0 J/(kg·K) | Typical for Titanium Alpha Beta Alloy | ||
Wärmeleitfähigkeit | 6.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.7 W/(m·K) | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Elektrisch
Property | Value | Related Standards | Shape |
---|---|---|---|
spezifischer Widerstand | 1.8000000000000001e-06 Ω·m Show Material materials with spezifischer Widerstand of 1.8000000000000001e-06 Ω·m | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.75 % Show Material materials with Aluminium of 5.5 - 6.75 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Sauerstoff | 0.2 % Show Material materials with Sauerstoff of 0.2 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Stickstoff | 0.05 % Show Material materials with Stickstoff of 0.05 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Wasserstoff | 0.0125 % Show Material materials with Wasserstoff of 0.0125 % | AMS 4928R, ASTM B348, AMS 4928, AMS 4967 | Bar |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Compressor blades, discs and rings for jet engines, airframe components, fasteners, rocket engine cases, helicopter rotor blades and critical forgings;Offshore & marine: Offshore tubulars and oil and gas equipment;Other: Biomedical implants and chemical processing equipment | |
Corrosion properties | Good corrosion resistance |