Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.28 g/cm³ Show Material materials with Dichte of 10.28 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.13 - 3.18 mm Show Material materials with Dicke of 0.13 - 3.18 mm |
Dimensions | Available thicknesses: 0.13mm, 0.18mm, 0.25mm, 0.38mm, 0.51mm, 0.64mm, 0.76mm, 1.02mm, 5.08mm, 0.64mm, 0.76mm, 1.02mm, 1.27mm, 1.52mm, 1.59mm, 2.03mm, 2.29mm, 3.18mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % | in 1 in. |
Elastizitätsmodul | 23.0 °C | 320 GPa Show Material materials with Elastizitätsmodul of 320 GPa | |
Härte, Vickers | 23.0 °C | 220 [-] Show Material materials with Härte, Vickers of 220 [-] | |
Zugfestigkeit | 20.0 °C | 1035 MPa Show Material materials with Zugfestigkeit of 1035 MPa | |
500.0 °C | 515 MPa Show Material materials with Zugfestigkeit of 515 MPa | ||
1000.0 °C | 175 MPa Show Material materials with Zugfestigkeit of 175 MPa | ||
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.8E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4.8E-6 1/K |
Kristallisationstemperatur | 1100 °C Show Material materials with Kristallisationstemperatur of 1100 °C | |
Schmelzpunkt | 2623 °C Show Material materials with Schmelzpunkt of 2623 °C | |
Spezifische Wärmekapazität | 23.0 °C | 259 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 259 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 142 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 142 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 200.0 °C | 5.34E-8 Ω·m Show Material materials with spezifischer Widerstand of 5.34E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Molybdän | 99.97 % Show Material materials with Molybdän of 99.97 % | min |
Technological properties
Property | ||
---|---|---|
Application areas | In the missile industry Molybdenum is used for nose cones, high temperature structural parts, nozzles, leading edges of control surfaces, support vanes, re-entry cones, and heat radiation shields. In electronics Molybdenum is used for cathodes, magnetron end hats, x-ray tube components, filaments, and glass-to-metal seals. In high-temperature applications Molybdenum is used for: furnace windings, structural furnace members, and containers for components exposed to high temperatures. |