Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.05 g/cm³ Show Material materials with Dichte of 8.05 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 609.6 mm Show Material materials with Breite of 609.6 mm |
Dicke | 0.76 - 3.18 mm Show Material materials with Dicke of 0.76 - 3.18 mm |
Länge | 1828 mm Show Material materials with Länge of 1828 mm |
Dimensions | Available thicknesses: 0.8mm, 1.0mm, 1.6mm, 2.5mm, 3.2mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 34 % Show Material materials with Dehnung of 34 % | in 2 in. |
Elastizitätsmodul | 23.0 °C | 141 GPa Show Material materials with Elastizitätsmodul of 141 GPa | |
Härte, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Härte, Rockwell B of 80 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | |
Streckgrenze | 23.0 °C | 276 MPa Show Material materials with Streckgrenze of 276 MPa | |
Zugfestigkeit | 23.0 °C | 518 MPa Show Material materials with Zugfestigkeit of 518 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.9E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-6 1/K | from 20°C to the mentioned temperature |
150.0 °C | 2.4E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-6 1/K | from 20°C to the mentioned temperature | |
200.0 °C | 3E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3E-6 1/K | from 20°C to the mentioned temperature | |
250.0 °C | 4.4E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4.4E-6 1/K | from 20°C to the mentioned temperature | |
300.0 °C | 6.1E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.1E-6 1/K | from 20°C to the mentioned temperature | |
350.0 °C | 7.5E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.5E-6 1/K | from 20°C to the mentioned temperature | |
400.0 °C | 8.7E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.7E-6 1/K | from 20°C to the mentioned temperature | |
450.0 °C | 8.9E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.9E-6 1/K | from 20°C to the mentioned temperature | |
500.0 °C | 1.05E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.05E-5 1/K | from 20°C to the mentioned temperature | |
600.0 °C | 1.18E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.18E-5 1/K | from 20°C to the mentioned temperature | |
Schmelzpunkt | 1427 °C Show Material materials with Schmelzpunkt of 1427 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 502 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 10 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 8.2E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.2E-7 Ω·m |
Magnetisch
Property | Value |
---|---|
Curie-Temperatur | 279 °C Show Material materials with Curie-Temperatur of 279 °C |
Chemical properties
Property | Value |
---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Eisen | Balance |
Kobalt | 0.5 % Show Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Nickel | 36 % Show Material materials with Nickel of 36 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Positioning devices • Bimetal thermostats • Advanced composite molds for aerospace industry • Dimensionally stable instruments and optical devices • Containers for LNG tankers • Transfer lines for LNG • Echo boxes and filters for mobile telephones • Magnetic shielding • Small electrical transformers • Metrology devices • Scientific instruments • Electrical circuit breakers • Temperature regulators • Clock balance wheels • Pendulum clocks • Precision condenser blades • Radar and microwave cavity resonators • Special electronic housings • Seals, spacers, and specialized frames • High voltage transmission lines • CRT applications: shadow masks, deflection clips, and electron gun components. |