Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.89 g/cm³ Show Material materials with Dichte of 8.89 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 3.18 - 57.2 mm Show Material materials with Breite of 3.18 - 57.2 mm |
Dimensions | Available widths: 3.2mm, 4.8mm, 6.4mm, 7.9mm, 9.5mm, 12.7mm, 15.9mm, 19.1mm, 22.2mm, 28.6mm, 31.8mm, 44.5mm, 50.8mm, 57.2mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | in 2 in. |
Elastizitätsmodul | 23.0 °C | 207 GPa Show Material materials with Elastizitätsmodul of 207 GPa | |
Härte, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Härte, Rockwell B of 80 [-] | |
Streckgrenze | 23.0 °C | 138 MPa Show Material materials with Streckgrenze of 138 MPa | |
Zugfestigkeit | 23.0 °C | 449 MPa Show Material materials with Zugfestigkeit of 449 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | from 30°C to the mentioned temperature |
Schmelzpunkt | 1440 °C Show Material materials with Schmelzpunkt of 1440 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 452 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 452 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 79 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 79 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-8 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-8 Ω·m |
Magnetisch
Property | Value |
---|---|
Curie-Temperatur | 360 °C Show Material materials with Curie-Temperatur of 360 °C |
Chemical properties
Property | Value |
---|---|
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Nickel | 99.5 % Show Material materials with Nickel of 99.5 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Nickel 201: Getter tabs, heating element sheathing, anodes, fuel cells, special purpose electron tubes, transistor enclosures, cathode shields, spark gaps |