Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18 g/cm³ Show Material materials with Dichte of 18 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 1 % Show Material materials with Dehnung of 1 % |
Elastizitätsmodul | 23.0 °C | 345 GPa Show Material materials with Elastizitätsmodul of 345 GPa |
Härte, Rockwell C | 23.0 °C | 34 [-] Show Material materials with Härte, Rockwell C of 34 [-] |
Streckgrenze | 23.0 °C | 517 MPa Show Material materials with Streckgrenze of 517 MPa |
Zugfestigkeit | 23.0 °C | 648 MPa Show Material materials with Zugfestigkeit of 648 MPa |
Chemical properties
Property | Value |
---|---|
Wolfram | 95 % Show Material materials with Wolfram of 95 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Tungsten Alloys: Radiation shielding, boring bars, counterweights in aircraft and racing cars |