Abmessung
Property | Value |
---|---|
Dicke | 0.05 mm Show Material materials with Dicke of 0.05 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 150 % Show Material materials with Dehnung of 150 % | ISO 527 |
Dehnung, transversal | 23.0 °C | 150 % Show Material materials with Dehnung, transversal of 150 % | ISO 527 |
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527 |
Elastizitätsmodul, transversal | 23.0 °C | 2.5 GPa Show Material materials with Elastizitätsmodul, transversal of 2.5 GPa | ISO 527 |
Zugfestigkeit | 23.0 °C | 130 MPa Show Material materials with Zugfestigkeit of 130 MPa | ISO 527 |
Zugfestigkeit, transversal | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit, transversal of 120 MPa | ISO 527 |
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders | |
Certifications | APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant. | |
Other | The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. |