Abmessung
Property | Value |
---|---|
Dicke | 0.03 mm Show Material materials with Dicke of 0.03 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 10 % Show Material materials with Dehnung of 10 % | ISO 527 |
Dehnung, transversal | 23.0 °C | 10 % Show Material materials with Dehnung, transversal of 10 % | ISO 527 |
Elastizitätsmodul | 23.0 °C | 5.5 GPa Show Material materials with Elastizitätsmodul of 5.5 GPa | ISO 527 |
Elastizitätsmodul, transversal | 23.0 °C | 4.5 GPa Show Material materials with Elastizitätsmodul, transversal of 4.5 GPa | ISO 527 |
Zugfestigkeit | 23.0 °C | 70 MPa Show Material materials with Zugfestigkeit of 70 MPa | ISO 527 |
Zugfestigkeit, transversal | 23.0 °C | 70 MPa Show Material materials with Zugfestigkeit, transversal of 70 MPa | ISO 527 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical insulation, printed circuit substrates, high temperature labels, flexible surface heaters, proven temperature resistance to use of lead free solders, acoustic speaker diaphragms, pressure sensor membranes | |
Certifications | APTIV® film is FDA and EU approved for food contact and is RoHS compliant. | |
Other | The key features are: High heat resistance, broad chemical resistance, excellent barrier properties, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. The APTIV 1100 series offers an improved thermal conductivity over APTIV 1000 films. | |
Processing methods | Can be laminated to other materials, thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. |