Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.26 g/cm³ Show Material materials with Dichte of 1.26 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.21 % Show Material materials with Wasserabsorption of 0.21 % | ISO 62 (50% RH, 24h) |
Abmessung
Property | Value |
---|---|
Dicke | 0.05 mm Show Material materials with Dicke of 0.05 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 200 % Show Material materials with Dehnung of 200 % | ISO 527 |
Dehnung, transversal | 23.0 °C | 200 % Show Material materials with Dehnung, transversal of 200 % | ISO 527 |
Durchschlagfestigkeit | 23.0 °C | 470 kJ/m² Show Material materials with Durchschlagfestigkeit of 470 kJ/m² | Def Stan 81-75 |
Elastizitätsmodul | 23.0 °C | 1.8 GPa Show Material materials with Elastizitätsmodul of 1.8 GPa | ISO 527 |
Elastizitätsmodul, transversal | 23.0 °C | 1.8 GPa Show Material materials with Elastizitätsmodul, transversal of 1.8 GPa | ISO 527 |
Reißfestigkeit | 23.0 °C | 6 kN/m Show Material materials with Reißfestigkeit of 6 kN/m | ISO 6383-1 |
Reißfestigkeit, transversal | 23.0 °C | 6 kN/m Show Material materials with Reißfestigkeit, transversal of 6 kN/m | ISO 6383-1 |
Zugfestigkeit | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit of 120 MPa | ISO 527 |
Zugfestigkeit, transversal | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit, transversal of 120 MPa | ISO 527 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 3 [-] Show Material materials with Dielektrizitätskonstante of 3 [-] | ASTM D150 (10MHz) |
Durchschlagfestigkeit | 23.0 °C | 190 kV/mm Show Material materials with Durchschlagfestigkeit of 190 kV/mm | ASTM D149 (6.25mm electrode) |
Durchschlagspannung | 23.0 °C | 9.5 kV Show Material materials with Durchschlagspannung of 9.5 kV | ASTM D149 (6.25mm electrode) |
Verlustfaktor | 23.0 °C | 3E-3 [-] Show Material materials with Verlustfaktor of 3E-3 [-] | ASTM D150 (10Mhz) |
spezifischer Widerstand | 23.0 °C | 2.00E+14 Ω·m Show Material materials with spezifischer Widerstand of 2.00E+14 Ω·m | ASTM D257 (100V) |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites | |
Certifications | APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21. | |
Other | The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing |