Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.4 g/cm³ Show Material materials with Dichte of 7.4 g/cm³ |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 232 °C Show Material materials with Schmelzpunkt of 232 °C |
Chemical properties
Property | Value |
---|---|
Chrom | 2 - 6 % Show Material materials with Chrom of 2 - 6 % |
Kupfer | 0.01 - 1 % Show Material materials with Kupfer of 0.01 - 1 % |
Silber | 3 - 5 % Show Material materials with Silber of 3 - 5 % |
Zinn | 90 - 100 % Show Material materials with Zinn of 90 - 100 % |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Other | The key features are: Excellent flow, good wetting of surfaces to be joined, electrically and thermally conductive, aluminium to aluminium can be soldered without using flux, carbon can be soldered to metals (e.g. copper, aluminium), ceramics and glass materials, C-Solder is not affected by cleaning solvents, C-Solder does not leave residues, C-Solder is not flammable, C-Solder is flux free, C-Solder is lead free |