Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.8 g/cm³ Show Material materials with Dichte of 1.8 g/cm³ | SRM 15 (typical fibre properties) |
Ertrag 12K | 23.0 °C | 800 mg/m Show Material materials with Ertrag 12K of 800 mg/m | SRM 13 |
Ertrag 24K | 23.0 °C | 1600 mg/m Show Material materials with Ertrag 24K of 1600 mg/m | SRM 13 |
Abmessung
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 1745 MPa Show Material materials with Biegefestigkeit of 1745 MPa | ASTM D790 (L/D=32, Vf=61%) |
Biegefestigkeit, transversal | 23.0 °C | 102 MPa Show Material materials with Biegefestigkeit, transversal of 102 MPa | ASTM D790 (L/D=32, Vf=61%) |
Biegemodul | 23.0 °C | 132 GPa Show Material materials with Biegemodul of 132 GPa | ASTM D790 (L/D=32, Vf=61%) |
Biegemodul, transversal | 23.0 °C | 8.8 GPa Show Material materials with Biegemodul, transversal of 8.8 GPa | ASTM D790 (L/D=32, Vf=61%) |
Druckfestigkeit | 23.0 °C | 1365 MPa Show Material materials with Druckfestigkeit of 1365 MPa | ASTM D3039 |
Druckfestigkeit, transversal | 23.0 °C | 196 MPa Show Material materials with Druckfestigkeit, transversal of 196 MPa | ASTM D3039 |
Elastizitätsmodul | 23.0 °C | 137 GPa Show Material materials with Elastizitätsmodul of 137 GPa | ASTM D3039 |
Elastizitätsmodul, transversal | 23.0 °C | 9.2 GPa Show Material materials with Elastizitätsmodul, transversal of 9.2 GPa | ASTM D3039 |
Interlaminare Scherfestigkeit | 23.0 °C | 97 MPa Show Material materials with Interlaminare Scherfestigkeit of 97 MPa | ASTM D2344 (L/D=4, Vf=59%) |
Kompressionsmodul | 23.0 °C | 127 MPa Show Material materials with Kompressionsmodul of 127 MPa | ASTM D3039 |
Kompressionsmodule, transversal | 23.0 °C | 10.2 MPa Show Material materials with Kompressionsmodule, transversal of 10.2 MPa | ASTM D3039 |
Schlepp-Zugkraft | 23.0 °C | 4830 MPa Show Material materials with Schlepp-Zugkraft of 4830 MPa | SRM 16 (typical fibre properties) |
Schlepp-Zugmodul | 23.0 °C | 234 GPa Show Material materials with Schlepp-Zugmodul of 234 GPa | SRM 16 (typical fibre properties) |
Zugfestigkeit | 23.0 °C | 2572 MPa Show Material materials with Zugfestigkeit of 2572 MPa | ASTM D3039 |
Zugfestigkeit, transversal | 23.0 °C | 81 MPa Show Material materials with Zugfestigkeit, transversal of 81 MPa | ASTM D3039 |
Technological properties
Property | ||
---|---|---|
Processing history | Epoxy sized 1.2% |