Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Oxidationsrate | 500.0 °C | 0.75 g/m²·h Show Material materials with Oxidationsrate of 0.75 g/m²·h | |
700.0 °C | 130 g/m²·h Show Material materials with Oxidationsrate of 130 g/m²·h | ||
Schüttdichte | 23.0 °C | 1.12 g/cm³ Show Material materials with Schüttdichte of 1.12 g/cm³ | ASTM F-1315 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Druckfestigkeit | 23.0 °C | 165 MPa Show Material materials with Druckfestigkeit of 165 MPa | ASTM C-695 |
Kompressionsmodul | 23.0 °C | 190 MPa Show Material materials with Kompressionsmodul of 190 MPa | |
Schlepp-Zugkraft | 23.0 °C | 190 MPa Show Material materials with Schlepp-Zugkraft of 190 MPa | |
Zugfestigkeit | 23.0 °C | 5.2 MPa Show Material materials with Zugfestigkeit of 5.2 MPa | ASTM F-152 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8E-8 Ω·m Show Material materials with spezifischer Widerstand of 8E-8 Ω·m | ASTM C-611 |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Flexible Graphite has unique physical and chemical properties that make it ideal for sealing and for high-temperature applications, such as thermal radiation shielding. Flexible graphite is a distinctive material with the essential characteristics of graphite plus some unique properties which make it a valuable material for packings and gaskets. |