Allgemein
Property | Value |
---|---|
Domänengröße | 10 - 20 μm Show Material materials with Domänengröße of 10 - 20 μm |
Substrat | PET, 188µm |
Abmessung
Elektrisch
Property | Temperature | Value |
---|---|---|
Ladungsträgermobilität | 23.0 °C | 3500 cm²/Vs Show Material materials with Ladungsträgermobilität of 3500 cm²/Vs |
Surface resistivity | 23.0 °C | 250 - 400 Ω/sq Show Material materials with Surface resistivity of 250 - 400 Ω/sq |
Optisch
Property | Value |
---|---|
Lichttransmission | 97 [-] Show Material materials with Lichttransmission of 97 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Light flexible displays, plastic electronics, printed circuit boards, liquid crystal displays, thin film photovoltaics, e-paper, sensors and OLEDs | |
Processing history | Growth method: CVD |