Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient hygroskopischer Ausdehnung | 23.0 °C | 5E-6 % Show Material materials with Koeffizient hygroskopischer Ausdehnung of 5E-6 % | |
Permeabilitätskoeffizient | 23.0 °C | 13 cm²/s Show Material materials with Permeabilitätskoeffizient of 13 cm²/s | E96 |
Sauerstoffindex | 23.0 °C | 25 % Show Material materials with Sauerstoffindex of 25 % | D2863-77 |
Wasserabsorption | 23.0 °C | 0.4 % Show Material materials with Wasserabsorption of 0.4 % | 24h |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 240 % Show Material materials with Dehnung of 240 % | D882-67 |
Dehnung, transversal | 23.0 °C | 240 % Show Material materials with Dehnung, transversal of 240 % | D882-67 |
Zugfestigkeit | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit of 120 MPa | D882-67 |
Zugfestigkeit, transversal | 23.0 °C | 120 MPa Show Material materials with Zugfestigkeit, transversal of 120 MPa | D882-67 |
Thermisch
Property | Temperature | Value | |
---|---|---|---|
Glasübergangstemperatur | 143 °C Show Material materials with Glasübergangstemperatur of 143 °C | ||
Koeffizient der thermischen Ausdehnung | 110.0 °C | 4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4E-5 1/K | |
Max. Betriebstemperatur, lang | 250 °C Show Material materials with Max. Betriebstemperatur, lang of 250 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 1450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1450 J/(kg·K) | |
Entflammbarkeit | UL94 VTM -1 (100 micron) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 25.0 °C | 3.3 [-] Show Material materials with Dielektrizitätskonstante of 3.3 [-] | at 50Hz, D150 |
Dissipation factor, 50Hz | 25.0 °C | 1.8E-3 [-] Show Material materials with Dissipation factor, 50Hz of 1.8E-3 [-] | D150 |
100.0 °C | 1.6E-3 [-] Show Material materials with Dissipation factor, 50Hz of 1.6E-3 [-] | D150 | |
Durchschlagfestigkeit | 23.0 °C | 128 kV/mm Show Material materials with Durchschlagfestigkeit of 128 kV/mm | D194-64 |
spezifischer Widerstand | 25.0 °C | 1.00E+15 Ω·m Show Material materials with spezifischer Widerstand of 1.00E+15 Ω·m | D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Other | “Stabar” K200 film offers an excellent combination of properties including: Intrinsic long term heat stability; Low flammability and extremely low smoke and toxic gas evolution on burning; Resistance to attack by a wide range of organic and inorganic chemicals and solvents; Low water absorption and good hydrolysis resistance at high temperatures and pressures; Resistance to radiation (X-rays, beta-rays and gamma rays) is amongst the best of thermoplastic materials; Good tear and fatigue resistance; Retention of good electrical properties over a wide temperature range. | |
Processing methods | “Stabar” K200 film can be adhesion-bonded either to itself or to other substrates, the bond strengths being dependent upon the type of adhesive and the surface preparation. “Stabar” K200 film may be fusion- bonded to itself, to reinforcements and to other substrates by application of heat and pressure. “Stabar” K200 film can be metallised by vacuum deposition and sputtering techniques, and is compatible with a range of inks and lacquers. |