Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 1.2 MPa Show Material materials with Druckfestigkeit of 1.2 MPa |
Kompressionsmodul | 23.0 °C | 75 MPa Show Material materials with Kompressionsmodul of 75 MPa |
Scherfestigkeit, L-Richtung | 23.0 °C | 0.7 MPa Show Material materials with Scherfestigkeit, L-Richtung of 0.7 MPa |
Scherfestigkeit, W-Richtung | 23.0 °C | 0.4 MPa Show Material materials with Scherfestigkeit, W-Richtung of 0.4 MPa |
Schubmodule, L-Richtung | 23.0 °C | 29 MPa Show Material materials with Schubmodule, L-Richtung of 29 MPa |
Schubmodule, W-Richtung | 23.0 °C | 19 MPa Show Material materials with Schubmodule, W-Richtung of 19 MPa |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace applications: Helicopter blades, fairings, interior panels, flooring, control surfaces, flaps, engine nacelles; HexWeb A1 honeycomb is qualified to all major aerospace specifications. Industrial applications: Marine and ground transportation, interior panels, flooring, bulkheads, hatches; racing boat shells; high performance car chassis and body panels; precision optical equipment; desiccant and filtration systems; radar reflectors, covers and emitters. | |
Other | The key features are: Outstanding resistance to corrosive attack by chemicals, high mechanical strength at low densities, fire retardant and self-extinguishing, excellent resistance to impact damage and moisture, low smoke and toxic gas emission, highly resistant to fungal growth, good dielectric properties, transparent radio and radar waves, low thermal conductivity |