Allgemein
Property | Value |
---|---|
Porosität | 1.8 - 2 % Show Material materials with Porosität of 1.8 - 2 % |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 11.3 - 15.8 MPa Show Material materials with Biegefestigkeit of 11.3 - 15.8 MPa |
Härte, Mohs | 23.0 °C | 2.5 [-] Show Material materials with Härte, Mohs of 2.5 [-] |
Zugfestigkeit | 23.0 °C | 10.3 MPa Show Material materials with Zugfestigkeit of 10.3 MPa |
Technological properties
Property | ||
---|---|---|
Chemical composition | Silica - 56.8%, Alumina - 33.37%, Ferric oxide - 0.79%, Titanium Dioxide - 2.42%, Calcium Oxide - 0.29%, Magnesium Oxide - 0.24% | |
Color | Grey | |
Other | Typical characteristics of the Pyrophyllite material include: Machinable, thermally insulating, good thermal shock properties, good mechanical stability once fired |