Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Multi Wall Carbon Nanotubes “Chunky” Powder NC006060 (>90% purity)
Free Standing aligned CNT arrays (Carpets) are synthesized by floating catalyst CVD method within a horizontal quartz reaction tube.
The CNT synthesis parameters are carefully selected to provide maximum-yield of CNT growth, high packing density as well as high graphitization level.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationAllgemein
Property | Value |
---|---|
Graphitierungsgrad | 0.3 - 0.4 [-] Show Material materials with Graphitierungsgrad of 0.3 - 0.4 [-] |
Abmessung
Property | Value |
---|---|
Länge der Nanoröhrchen | 300 - 1000 µm Show Material materials with Länge der Nanoröhrchen of 300 - 1000 µm |
Nanoröhrendurchmesser | 30 - 90 nm Show Material materials with Nanoröhrendurchmesser of 30 - 90 nm |
Thermisch
Property | Value |
---|---|
Oxidierungsschwelle | 600 - 700 °C Show Material materials with Oxidierungsschwelle of 600 - 700 °C |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.