Allgemein
Property | Value |
---|---|
Bio-based content | 100 % Show Material materials with Bio-based content of 100 % |
Dichte | 1.26 g/cm³ Show Material materials with Dichte of 1.26 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 80.0 MPa Show Material materials with Biegefestigkeit of 80.0 MPa |
Biegemodul | 2.38 GPa Show Material materials with Biegemodul of 2.38 GPa |
Dehnung | 3.0 % Show Material materials with Dehnung of 3.0 % |
Härte, Shore D | 69.0 [-] Show Material materials with Härte, Shore D of 69.0 [-] |
Impact strength, Izod unnotched, ASTM | 8.0 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 8.0 J/m |
Zugfestigkeit | 54 MPa Show Material materials with Zugfestigkeit of 54 MPa |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 60 g/10min Show Material materials with Schmelzmassenflussrate of 60 g/10min | 210°C/2.16kg |
80 g/10min Show Material materials with Schmelzmassenflussrate of 80 g/10min | 210°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Molded products, cutleries, tableware (<100°C) | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Clean extruder with general purpose polypropylene or polystyrene. 2. Vacuum out hopper system to avoid contamination and make sure that the humidity of the air is below 40°C at dew point. 3. Introduce ICBP Bio Resin in to the extruder at the operating conditions used in the first step. 4. Once ICBP Bio Resin has been purged, reduce barrel temperatures to desired set points. 5. At shutdown, purge machine with PP or PS. |