Allgemein
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 14.0 MPa Show Material materials with Biegefestigkeit of 14.0 MPa |
Biegemodul | 4.43 GPa Show Material materials with Biegemodul of 4.43 GPa |
Dehnung | 89.0 % Show Material materials with Dehnung of 89.0 % |
Härte, Shore D | 64.0 [-] Show Material materials with Härte, Shore D of 64.0 [-] |
Impact strength, Izod unnotched, ASTM | 38.0 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 38.0 J/m |
Zugfestigkeit | 9 MPa Show Material materials with Zugfestigkeit of 9 MPa |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 9 g/10min Show Material materials with Schmelzmassenflussrate of 9 g/10min | 175°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Toy, tube, profile extrusion | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Clean extruder with general purpose polyethylene or polypropylene. 2. Vacuum out hopper system to avoid contamination and make sure that the humidity of the air is below 40°C at dew point. 3. Introduce ICBP Bio Resin in to the extruder at the operating conditions used in the first step. 4. Once ICBP Bio Resin has been purged, reduce barrel temperatures to desired set points. 5. At shutdown, purge machine with PE or PP. |