Allgemein
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 65.0 MPa Show Material materials with Biegefestigkeit of 65.0 MPa |
Biegemodul | 2.0 GPa Show Material materials with Biegemodul of 2.0 GPa |
Dehnung | 30.0 % Show Material materials with Dehnung of 30.0 % |
Härte, Shore D | 70.0 [-] Show Material materials with Härte, Shore D of 70.0 [-] |
Impact strength, Izod unnotched, ASTM | 20.0 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 20.0 J/m |
Zugfestigkeit | 40 MPa Show Material materials with Zugfestigkeit of 40 MPa |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 8 g/10min Show Material materials with Schmelzmassenflussrate of 8 g/10min | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Straw, tube | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Purge the machine using LDPE/HDPE material at original processing temperature. 2. Lower the temperature to 130 -150°C. 3. Purge the ICBP Bio Resin EVO grade at temperature of 125 - 145°C. 4. Properly adjust according to the conditions of machine and finished product. |