Allgemein
Property | Value |
---|---|
Bio-based content | 100 % Show Material materials with Bio-based content of 100 % |
Dichte | 1.26 - 1.3 g/cm³ Show Material materials with Dichte of 1.26 - 1.3 g/cm³ |
Mechanisch
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 110.0 - 120.0 °C Show Material materials with Schmelzpunkt of 110.0 - 120.0 °C |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 5 g/10min Show Material materials with Schmelzmassenflussrate of 5 g/10min | 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Shopping bag, garbage bag, mulch film, waste bag, food packaging bag | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Pre-clean the machine with LDPE at original processing temperature. 2. Purge the machine using BMF 990 at temperature 140-160°C. 3. Barrel temperature should be lowered if the die temperature is too high or the viscosity of the extruded material is too thin. 4. Adjust the cooling air volume to make the bubble smooth and steady. |