Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Druckfestigkeit | 23.0 °C | 802 MPa Show Material materials with Druckfestigkeit of 802 MPa | ASTM D6641, Lamina |
Elastizitätsmodul | 23.0 °C | 60 GPa Show Material materials with Elastizitätsmodul of 60 GPa | ASTM D3039, Lamina |
Kompressionsmodul | 23.0 °C | 71 MPa Show Material materials with Kompressionsmodul of 71 MPa | ASTM D695, Lamina |
Shear modulus, G₁₂ | 23.0 °C | 5.7 GPa Show Material materials with Shear modulus, G₁₂ of 5.7 GPa | ASTM D5379, Lamina |
Shear strength, τ₁₂ | 23.0 °C | 126 MPa Show Material materials with Shear strength, τ₁₂ of 126 MPa | |
Shear strength, τ₁₃ | 23.0 °C | 79 MPa Show Material materials with Shear strength, τ₁₃ of 79 MPa | ASTM D2344, Lamina |
Shear strength, τ₁₃ laminate | 25.0 °C | 66 MPa Show Material materials with Shear strength, τ₁₃ laminate of 66 MPa | |
85.0 °C | 59 MPa Show Material materials with Shear strength, τ₁₃ laminate of 59 MPa | ||
Tensile strength laminate | 25.0 °C | 668 MPa Show Material materials with Tensile strength laminate of 668 MPa | |
85.0 °C | 670 MPa Show Material materials with Tensile strength laminate of 670 MPa | ||
Zugfestigkeit | 23.0 °C | 871 MPa Show Material materials with Zugfestigkeit of 871 MPa | ASTM D3039, Lamina |
Technological properties
Property | ||
---|---|---|
Application areas | Marine: The shells of boats and sport catamarans can be made of composites;Car tuning: The composite material provides solutions for automotive parts to be light-weighted, stylish and aesthetic;Sports equipment: Frame, wheels, seat, seat post, handlebar, head stem and crank arm of a sports bicycle are made of carbon composite | |
Processing history | Reinforcing filler: carbon fabric 22508 (twill 2x2, 200 g/m2, HTA40). Carbon plastic is produced by vacuum molding. | |
Processing methods | Holding at a temperature of 25-30°C, for 12 hours, a vacuum of -1 bar. Heating 2°C/min. up to 120°C, holding at 120°C for 180 minutes. Heating 2°C/min. up to 180°C, holding at 180°C for 180 minutes, cooling no faster than 5°C/min. up to 50°С. |