Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit 180°, in longitudinaler Richtung | 23.0 °C | 3 [-] Show Material materials with Biegefestigkeit 180°, in longitudinaler Richtung of 3 [-] | r = x t, t <0.5mm |
Biegefähigkeit 180°, in transversaler Richtung | 23.0 °C | 2.5 [-] Show Material materials with Biegefähigkeit 180°, in transversaler Richtung of 2.5 [-] | r = x t, t <0.5mm |
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 2 [-] Show Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 2 [-] | r = x t, t <0.5mm |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 2 [-] Show Material materials with Biegefähigkeit 90°, in transversaler Richtung of 2 [-] | r = x t, t <0.5mm |
Dehnung A50 | 23.0 °C | 4 % Show Material materials with Dehnung A50 of 4 % | |
Elastizitätsmodul | 23.0 °C | 137 GPa Show Material materials with Elastizitätsmodul of 137 GPa | cold formed |
Härte, Vickers | 23.0 °C | 160 - 200 [-] Show Material materials with Härte, Vickers of 160 - 200 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 500 MPa Show Material materials with Streckgrenze Rp 0,2 of 500 MPa | |
Zugfestigkeit | 23.0 °C | 540 - 630 MPa Show Material materials with Zugfestigkeit of 540 - 630 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 20°C to the mentioned temperature |
Spezifische Wärmekapazität | 23.0 °C | 381 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 381 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 330 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 330 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+7 - 5.20E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+7 - 5.20E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 0.2 - 1.2 % Show Material materials with Chrom of 0.2 - 1.2 % | ||
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % | max. | |
Kupfer | Balance | ||
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | max. | |
Zirkonium | 0.05 - 0.25 % Show Material materials with Zirkonium of 0.05 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Hybrid Cars. Electrical: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Components for the electrical industry, Stamped parts, Semiconductor Components, Junction Boxes, Photovoltaic Systems. | |
Brazing | Excellent | |
Cold Forming | Good | |
Corrosion properties | STOL® 95 is resistant to pure water vapour and non oxidizingacids and alkalis as well as neutral saline solutions. The material is insensitive to stress corrosion cracking. | |
Heat Treatment | Temper: R540 | |
Machining | Rating 20, less suitable | |
Other | This alloy is in accordance with RoHS 2002/96/CE for electric & electronic equipments and 2002/53/CE for automotive industry. It is suitable for high voltage applications as hybrid cars or photovoltaics. | |
Plating | Electroplating is excellent | |
Welding | Gas Shielded Arc Welding: Excellent, Laser Welding: Fair |