Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 0.91 g/cm³ Show Material materials with Dichte of 0.91 g/cm³ | |
Filmstärke | 20.0 °C | 22.89 - 36.63 m²/kg Show Material materials with Filmstärke of 22.89 - 36.63 m²/kg | |
Oberflächendichte | 20.0 °C | 2.73E-3 - 4.37E-3 g/cm² Show Material materials with Oberflächendichte of 2.73E-3 - 4.37E-3 g/cm² | |
Schrumpfung | 120.0 °C | 4 % Show Material materials with Schrumpfung of 4 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Schrumpfung, diagonal | 120.0 °C | 2 % Show Material materials with Schrumpfung, diagonal of 2 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Abmessung
Property | Value |
---|---|
Dicke | 0.03 - 0.05 mm Show Material materials with Dicke of 0.03 - 0.05 mm |
Dimensions | Available thicknesses: 30, 35, 40, 48µm. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 200 % Show Material materials with Dehnung of 200 % | GOST 14236, ISO 527, ASTM D882 |
Dehnung, transversal | 20.0 °C | 70 % Show Material materials with Dehnung, transversal of 70 % | GOST 14236, ISO 527, ASTM D882 |
Zugfestigkeit | 20.0 °C | 140 MPa Show Material materials with Zugfestigkeit of 140 MPa | GOST 14236, ISO 527, ASTM D882 |
Zugfestigkeit, transversal | 20.0 °C | 280 MPa Show Material materials with Zugfestigkeit, transversal of 280 MPa | GOST 14236, ISO 527, ASTM D882 |
Optisch
Property | Value | Comment |
---|---|---|
Opazität | 2 % Show Material materials with Opazität of 2 % | GOST 15875, ISO 14782, ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality solvent based rotogravure and flexographic printing, for production of fully wrapped labels for bottles, for labeling with cold and hot melt glue, solvent based and solvent free lamination with polyurethane adhesives (if necessary). | |
Friction | Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | LGBA BOPP films comprise: A treated side of modified copolymer skin layer, a transparent biaxially oriented polypropylene; a glossy, none treated, Non-heat-sealable polypropylene skin layer with standard coefficient of friction. | |
Processing history | Treatment level: 38 mN/m (ISO 8296, ASTM D 2578). |