Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 0.91 g/cm³ Show Material materials with Dichte of 0.91 g/cm³ | |
Filmstärke | 20.0 °C | 27.5 - 54.9 m²/kg Show Material materials with Filmstärke of 27.5 - 54.9 m²/kg | |
Oberflächendichte | 20.0 °C | 1.82E-3 - 3.64E-3 g/cm² Show Material materials with Oberflächendichte of 1.82E-3 - 3.64E-3 g/cm² | |
Schrumpfung | 120.0 °C | 4 % Show Material materials with Schrumpfung of 4 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Schrumpfung, diagonal | 120.0 °C | 2 % Show Material materials with Schrumpfung, diagonal of 2 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Abmessung
Property | Value |
---|---|
Dicke | 0.02 - 0.04 mm Show Material materials with Dicke of 0.02 - 0.04 mm |
Dimensions | Available thicknesses: 20, 25, 30, 35, 40µm. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 200 % Show Material materials with Dehnung of 200 % | GOST 14236, ISO 527, ASTM D882 |
Dehnung, transversal | 20.0 °C | 70 % Show Material materials with Dehnung, transversal of 70 % | GOST 14236, ISO 527, ASTM D882 |
Zugfestigkeit | 20.0 °C | 140 MPa Show Material materials with Zugfestigkeit of 140 MPa | GOST 14236, ISO 527, ASTM D882 |
Zugfestigkeit, transversal | 20.0 °C | 280 MPa Show Material materials with Zugfestigkeit, transversal of 280 MPa | GOST 14236, ISO 527, ASTM D882 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality rotogravure and flexographic solvent based printing; for lamination with solvent based or solventless polyurethane adhesives; production of decorative packaging for flowers, gift wrap and etc.; heat sealing by string is possible; lamination with films, paper and cardboard. | |
Friction | Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | PMD.M BOPP films comprise: An aluminum layer, a treated modified copolymer layer for aluminum adhesion, a transparent oriented polypropylene core layer, a non-heat-sealable skin layer with high coefficient of friction, without treatment. | |
Processing history | Treatment level: 36 mN/m (ISO 8296, ASTM D 2578). |