Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.51 g/cm³ Show Material materials with Dichte of 4.51 g/cm³ | Sheet, Plate |
Abmessung
Property | Value | Shape |
---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet |
600 mm Show Material materials with Breite of 600 mm | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | Plate | |
Länge | 1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Länge of 5000 mm | Sheet | |
6500 mm Show Material materials with Länge of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Shape | Comment |
---|---|---|---|
Elastizitätsmodul | 106.0 GPa Show Material materials with Elastizitätsmodul of 106.0 GPa | Sheet, Plate | |
Härte, Brinell | 200.0 Show Material materials with Härte, Brinell of 200.0 | Sheet, Plate | |
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium | |
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium | |
Streckgrenze | 485.0 MPa Show Material materials with Streckgrenze of 485.0 MPa | Sheet, Plate | |
Zugfestigkeit | 550.0 MPa Show Material materials with Zugfestigkeit of 550.0 MPa | Sheet, Plate |
Thermisch
Property | Value | Shape | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | |
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium | |
Spezifische Wärmekapazität | 540 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 540 J/(kg·K) | Sheet, Plate | |
Wärmeleitfähigkeit | 18 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18 W/(m·K) | Sheet, Plate |
Chemical properties
Property | Value | Shape |
---|---|---|
Eisen | 0.5 Show Material materials with Eisen of 0.5 | Sheet, Plate |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | Sheet, Plate |
Sauerstoff | 0.4 Show Material materials with Sauerstoff of 0.4 | Sheet, Plate |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Sheet, Plate |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | Sheet, Plate |