Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.5 g/cm³ Show Material materials with Dichte of 4.5 g/cm³ | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Abmessung
Property | Value | Related Standards | Shape |
---|---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet |
600 mm Show Material materials with Breite of 600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
Länge | 1500 mm Show Material materials with Länge of 1500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
5000 mm Show Material materials with Länge of 5000 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
6500 mm Show Material materials with Länge of 6500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastizitätsmodul | 108.0 GPa Show Material materials with Elastizitätsmodul of 108.0 GPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Härte, Brinell | 150.0 Show Material materials with Härte, Brinell of 150.0 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium | ||
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium | ||
Streckgrenze | 275.0 MPa Show Material materials with Streckgrenze of 275.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Zugfestigkeit | 345.0 MPa Show Material materials with Zugfestigkeit of 345.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium | ||
Spezifische Wärmekapazität | 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 520 J/(kg·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Wärmeleitfähigkeit | 17 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 17 W/(m·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.3 Show Material materials with Eisen of 0.3 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Palladium | 0.12 - 0.25 % Show Material materials with Palladium of 0.12 - 0.25 % | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Sauerstoff | 0.25 Show Material materials with Sauerstoff of 0.25 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Stickstoff | 0.03 Show Material materials with Stickstoff of 0.03 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |