Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.45 g/cm³ Show Material materials with Dichte of 4.45 g/cm³ | Sheet, Plate |
Abmessung
Property | Value | Shape |
---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet |
600 mm Show Material materials with Breite of 600 mm | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | Plate | |
Länge | 1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Länge of 5000 mm | Sheet | |
6500 mm Show Material materials with Länge of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Shape |
---|---|---|
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | Sheet, Plate |
Streckgrenze | 760.0 MPa Show Material materials with Streckgrenze of 760.0 MPa | Sheet, Plate |
Zugfestigkeit | 825.0 - 860.0 MPa Show Material materials with Zugfestigkeit of 825.0 - 860.0 MPa | Sheet, Plate |
Thermisch
Property | Value | Shape | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | |
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | |
Spezifische Wärmekapazität | 560 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 560 J/(kg·K) | Sheet, Plate | |
Wärmeleitfähigkeit | 6.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.9 W/(m·K) | Sheet, Plate |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | Sheet, Plate |
Eisen | 0.25 Show Material materials with Eisen of 0.25 | Sheet, Plate |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | Sheet, Plate |
Sauerstoff | 0.13 Show Material materials with Sauerstoff of 0.13 | Sheet, Plate |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Sheet, Plate |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Sheet, Plate |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | Sheet, Plate |