Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.428999999999999 g/cm³ Show Material materials with Dichte of 4.428999999999999 g/cm³ | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
4.43 g/cm³ Show Material materials with Dichte of 4.43 g/cm³ | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Abmessung
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet | ||
600 mm Show Material materials with Breite of 600 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Plate | |||
1524 mm Show Material materials with Breite of 1524 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet | |||
1600 mm Show Material materials with Breite of 1600 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Plate | |||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar | |
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Tube | ||
7 mm Show Material materials with Durchmesser of 7 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar | |||
25.4 mm Show Material materials with Durchmesser of 25.4 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet | |||
115 mm Show Material materials with Durchmesser of 115 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar | |||
125 mm Show Material materials with Durchmesser of 125 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet | |||
130 mm Show Material materials with Durchmesser of 130 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet, Tube | |||
350 mm Show Material materials with Durchmesser of 350 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet | |||
Länge | 1000 mm Show Material materials with Länge of 1000 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Tube | ||
1500 mm Show Material materials with Länge of 1500 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate | |||
3000 mm Show Material materials with Länge of 3000 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet | |||
4500 mm Show Material materials with Länge of 4500 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet | |||
5000 mm Show Material materials with Länge of 5000 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Tube | |||
6000 mm Show Material materials with Länge of 6000 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar | max | ||
6500 mm Show Material materials with Länge of 6500 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Plate | |||
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Tube | ||
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Billet |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Dehnung | 14.0 % Show Material materials with Dehnung of 14.0 % | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
Elastizitätsmodul | 110.0 - 119.0 GPa Show Material materials with Elastizitätsmodul of 110.0 - 119.0 GPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
114.0 GPa Show Material materials with Elastizitätsmodul of 114.0 GPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate | |
Härte, Brinell | 310.0 Show Material materials with Härte, Brinell of 310.0 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
334.0 Show Material materials with Härte, Brinell of 334.0 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate | |
Härte, Rockwell C | 36.0 Show Material materials with Härte, Rockwell C of 36.0 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
Härte, Vickers | 349.0 Show Material materials with Härte, Vickers of 349.0 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
Poissonzahl | 0.31 [-] Show Material materials with Poissonzahl of 0.31 [-] | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
Schubmodule | 40.0 GPa Show Material materials with Schubmodule of 40.0 GPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
Streckgrenze | 830.0 MPa Show Material materials with Streckgrenze of 830.0 MPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
880.0 MPa Show Material materials with Streckgrenze of 880.0 MPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate | |
Zugfestigkeit | 862.0 - 1200.0 MPa Show Material materials with Zugfestigkeit of 862.0 - 1200.0 MPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
895.0 MPa Show Material materials with Zugfestigkeit of 895.0 MPa | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | ||
Spezifische Wärmekapazität | 560 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 560 J/(kg·K) | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate | |
Wärmeleitfähigkeit | 7.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.1 W/(m·K) | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.75 % Show Material materials with Aluminium of 5.5 - 6.75 % | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
6.0 % Show Material materials with Aluminium of 6.0 % | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate | |
Eisen | 0.25 Show Material materials with Eisen of 0.25 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate |
0.3 Show Material materials with Eisen of 0.3 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate | |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Sauerstoff | 0.2 Show Material materials with Sauerstoff of 0.2 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate, Bar, Billet, Tube |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
4.0 % Show Material materials with Vanadium of 4.0 % | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Bar, Billet, Tube, Sheet, Plate | |
Wasserstoff | 0.0125 Show Material materials with Wasserstoff of 0.0125 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |
Yttrium | 0.005 Show Material materials with Yttrium of 0.005 | ASME SB-265, AMS 4911, ASME SB-348, AMS 4928, AMS 4965, AMS 4967 | Sheet, Plate |