Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.76 g/cm³ Show Material materials with Dichte of 4.76 g/cm³ | Sheet, Plate |
Abmessung
Property | Value | Shape |
---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet |
600 mm Show Material materials with Breite of 600 mm | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | Plate | |
Länge | 1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Länge of 5000 mm | Sheet | |
6500 mm Show Material materials with Länge of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Shape |
---|---|---|
Dehnung | 22.0 % Show Material materials with Dehnung of 22.0 % | Sheet, Plate |
Elastizitätsmodul | 82.0 GPa Show Material materials with Elastizitätsmodul of 82.0 GPa | Sheet, Plate |
Härte, Rockwell B | 95.0 Show Material materials with Härte, Rockwell B of 95.0 | Sheet, Plate |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Sheet, Plate |
Schubmodule | 30.8 GPa Show Material materials with Schubmodule of 30.8 GPa | Sheet, Plate |
Streckgrenze | 770.0 MPa Show Material materials with Streckgrenze of 770.0 MPa | Sheet, Plate |
Zugfestigkeit | 790.0 MPa Show Material materials with Zugfestigkeit of 790.0 MPa | Sheet, Plate |
Thermisch
Property | Value | Shape | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.099999999999997e-06 - 9.699999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.099999999999997e-06 - 9.699999999999999e-06 1/K | Typical for Titanium Beta Alloy | |
Schmelzpunkt | 1550.0 - 1815.0 °C Show Material materials with Schmelzpunkt of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Spezifische Wärmekapazität | 490.0 - 580.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 490.0 - 580.0 J/(kg·K) | Typical for Titanium Beta Alloy | |
Wärmeleitfähigkeit | 8.08 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8.08 W/(m·K) | Sheet, Plate |
Chemical properties