Allgemein
Property | Value | Shape | Related Standards |
---|---|---|---|
Dichte | 4.37 g/cm³ Show Material materials with Dichte of 4.37 g/cm³ | Bar, Billet | |
4.37 g/cm³ Show Material materials with Dichte of 4.37 g/cm³ | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Abmessung
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Durchmesser | 7 mm Show Material materials with Durchmesser of 7 mm | Bar | ||
115 mm Show Material materials with Durchmesser of 115 mm | Bar | |||
130 mm Show Material materials with Durchmesser of 130 mm | Billet | |||
350 mm Show Material materials with Durchmesser of 350 mm | Billet | |||
Länge | 3000 mm Show Material materials with Länge of 3000 mm | Billet | ||
4500 mm Show Material materials with Länge of 4500 mm | Billet | |||
6000 mm Show Material materials with Länge of 6000 mm | Bar | max |
Mechanisch
Property | Value | Shape | Related Standards |
---|---|---|---|
Dehnung | 10.0 % Show Material materials with Dehnung of 10.0 % | Bar, Billet | |
Elastizitätsmodul | 117.0 GPa Show Material materials with Elastizitätsmodul of 117.0 GPa | Bar, Billet | |
128 GPa Show Material materials with Elastizitätsmodul of 128 GPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Härte, Rockwell C | 36.0 [-] Show Material materials with Härte, Rockwell C of 36.0 [-] | Bar, Billet | |
Poissonzahl | 0.35 [-] Show Material materials with Poissonzahl of 0.35 [-] | Bar, Billet | |
Schlagfestigkeit, Charpy gekerbt | 20.0 - 34.0 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 20.0 - 34.0 kJ/m² | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | |
Schubmodule | 42.0 GPa Show Material materials with Schubmodule of 42.0 GPa | Bar, Billet | |
Streckgrenze | 827.0 MPa Show Material materials with Streckgrenze of 827.0 MPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | |
Zugfestigkeit | 897.0 MPa Show Material materials with Zugfestigkeit of 897.0 MPa | Bar, Billet | |
931.0 MPa Show Material materials with Zugfestigkeit of 931.0 MPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Thermisch
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 0.0000085 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000085 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | |
20 °C | 0.0000090 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000090 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
100 °C | 0.0000085 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000085 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
315 °C | 0.0000090 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000090 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Schmelzpunkt | 1538.0 °C Show Material materials with Schmelzpunkt of 1538.0 °C | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Spezifische Wärmekapazität | 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 502 J/(kg·K) | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Wärmeleitfähigkeit | 6 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6 W/(m·K) | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
6.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.5 W/(m·K) | Bar, Billet |
Elektrisch
Property | Value | Related Standards |
---|---|---|
spezifischer Widerstand | 1.9699999999999998e-06 Ω·m Show Material materials with spezifischer Widerstand of 1.9699999999999998e-06 Ω·m | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Chemical properties
Property | Value | Shape | Related Standards |
---|---|---|---|
Aluminium | 7.35 - 8.35 % Show Material materials with Aluminium of 7.35 - 8.35 % | Bar, Billet | |
7.5 - 8.5 % Show Material materials with Aluminium of 7.5 - 8.5 % | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Eisen | 0.3 Show Material materials with Eisen of 0.3 | Bar, Billet | |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Molybdän | 0.75 - 1.25 % Show Material materials with Molybdän of 0.75 - 1.25 % | Bar, Billet | |
0.75 - 1.75 % Show Material materials with Molybdän of 0.75 - 1.75 % | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Sauerstoff | 0.12 Show Material materials with Sauerstoff of 0.12 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Vanadium | 0.75 - 1.75 % Show Material materials with Vanadium of 0.75 - 1.75 % | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Wasserstoff | 0.0125 Show Material materials with Wasserstoff of 0.0125 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |