Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.5 g/cm³ Show Material materials with Dichte of 4.5 g/cm³ | Bar |
Abmessung
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Durchmesser | 7 mm Show Material materials with Durchmesser of 7 mm | Bar | ||
115 mm Show Material materials with Durchmesser of 115 mm | Bar | |||
Länge | 6000 mm Show Material materials with Länge of 6000 mm | Bar | max |
Mechanisch
Property | Value | Shape | Comment |
---|---|---|---|
Dehnung | 6.0 - 10.0 % Show Material materials with Dehnung of 6.0 - 10.0 % | Bar | |
Elastizitätsmodul | 100.0 - 120.0 GPa Show Material materials with Elastizitätsmodul of 100.0 - 120.0 GPa | Typical for Titanium Alpha Beta Alloy | |
Zugfestigkeit | 930.0 - 1230.0 MPa Show Material materials with Zugfestigkeit of 930.0 - 1230.0 MPa | Bar |
Thermisch
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | ||
Spezifische Wärmekapazität | 200 °C | 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 502 J/(kg·K) | Bar | |
Wärmeleitfähigkeit | 8.01 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8.01 W/(m·K) | Bar |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 5.5 - 7.0 % Show Material materials with Aluminium of 5.5 - 7.0 % | Bar |
Chrom | 0.8 - 2.0 % Show Material materials with Chrom of 0.8 - 2.0 % | Bar |
Eisen | 0.2 - 0.7 % Show Material materials with Eisen of 0.2 - 0.7 % | Bar |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | Bar |
Molybdän | 2.0 - 3.0 % Show Material materials with Molybdän of 2.0 - 3.0 % | Bar |
Sauerstoff | 0.15 Show Material materials with Sauerstoff of 0.15 | Bar |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | Bar |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Bar |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | Bar |
Zirkonium | 0.5 Show Material materials with Zirkonium of 0.5 | Bar |